Precious-metal alloys with crucible insert:
When the casting temperature is reached, it
must be maintained for several seconds before
the casting process is triggered (see table on
page 35). This holding time is absolutely nec-
essary to optimize the flow behaviour of the
alloy! Trigger the casting process when the
holding time has elapsed and the actual tem-
perature has reached the casting temperature.
The casting is carried out with overpressure.
Alloy, chamber pressure, casting temperature
and casting number are displayed during the
process.
14. Remove the mould.
15. Close the mould door. The casting process is
completed.
WARNINGS
Risk of burn injuries!
Use mould tongs!
Summary of Contents for 39701001
Page 1: ...Gerätedokumentation Miteinander zum Erfolg ...
Page 2: ......
Page 4: ......
Page 11: ...English Nautilus CC plus Nautilus T 7 86105 BA en 01 en Unpacking Packing REF 17909 ...
Page 47: ...Nautilus CC plus en English ...
Page 63: ...Nautilus T en English ...
Page 87: ...English Nautilus CC plus Nautilus T 83 86105 BA en 01 en NAUTILUS T bar ...
Page 89: ......
Page 90: ......
Page 91: ......
Page 92: ......
Page 93: ......