15
Step by step:
1. Using a 12mm drill (0.47”) make a 90mm deep hole. (Threaded bar M10);
2. Clean the hole with a blower or vacuum cleaner to remove the dust residue;
3. Place the threaded bar into the hole to measure the depth. The bar has a mark
that must be close to the floor/ground;
4. Place the HVU capsule into the hole;
5. Fasten the threaded bar to the drill and tighten it until it hits the bottom of the
hole or until the mark of the threaded bar is close to the floor/ground;
6. Use the drill until the chemical material rises to the surface;
7. Do not touch the threaded bar to allow time for the chemical reaction (10 min);
8. The curing time is according to the table:
Curing time under general conditions
Data according to ETA-05/0255/0256/0257, edition 2010-03-01 /
2006-01-20
Base material temperature
Curing time necessary for the fastening to
receive the tcu total load
20°C to 40°C
20 min
10°C to 19°C
30 min
0°C to 9°C
1 h
-5°C to - 1°C
5 h