General Maintenance Procedures
Page 19
Frettage
Corrosion set up by small relative movement of parts with no
lubrication.
Replace bearing. Clean all related parts. Check seals and check
for proper lubrication.
Heat Discoloration
Heat discoloration can range from faint yellow to dark blue
resulting from overload or incorrect lubrication.
Excessive heat can cause softening of races or rollers.
To check for loss of temper on races or rollers, a simple file test
may be made. A file drawn over a tempered part will grab and
cut metal, whereas a file drawn over a hard part will glide readily
with no metal cutting.
Replace bearing if overheating damage is indicated. Check
seals and other related parts for damage.
Stain Discoloration
Discoloration can range from light brown to black caused by
incorrect lubrication or moisture.
If the stain can be removed by light polishing or if no evidence of
overheating is visible, the bearing can be reused.
Check seals and other related parts for damage.
Figure 16
Figure 17
Figure 18
Summary of Contents for DX180LC
Page 1: ...Shop Manual K1015439E Serial Number 5001 and Up DX225LC ...
Page 5: ...1Safety ...
Page 7: ...Track Excavator Safety SP000014 Page 2 MEMO ...
Page 50: ...1Specifications ...
Page 73: ...1General Maintenance ...
Page 91: ...SP000017 Page 1 Standard Torques SP000017 STANDARD TORQUESSP000017 Standard Torques Edition 1 ...
Page 105: ...1Upper Structure ...
Page 106: ...Cabin Page 1 SP000943 SP000943 CABIN SP000943 Cabin Edition 1 ...
Page 110: ...Thank you very much for your reading Please Click Here Then Get More Information ...