98
Powermax125
Service Manual 808070
6 – Machine Torch Setup
FineCut – stainless steel
Air flow rate – slpm/scfh
Hot
217 / 460
Cold
226 / 480
Metric
Material
Thickness
Current
Torch-to-Work
Distance
Initial Pierce Height
Pierce Delay
Time
Recommended
Cut Speed
Voltage
mm
A
mm
mm
%
seconds
mm/min
volts
0.5
30
0.02
0.08
400
0.0
4825
77
0.6
4825
77
0.8
0.1
4825
73
1
40
0.2
4825
86
1.5
0.4
4825
72
2
45
4550
72
3
0.5
2335
70
4
995
72
English
Material
Thickness
Current
Torch-to-Work
Distance
Initial Pierce Height
Pierce Delay
Time
Recommended
Cut Speed
Voltage
inches
A
inches
inches
%
seconds
ipm
volts
26 GA
30
0.02
0.08
400
0.0
190
77
24 GA
190
77
22 GA
0.1
190
74
20 GA
190
72
18 GA
40
0.2
190
80
16 GA
0.4
190
72
14 GA
45
190
72
12 GA
0.5
110
70
10 GA
70
71