90
Powermax125
Service Manual 808070
6 – Machine Torch Setup
65 A shielded cutting – stainless steel
Air flow rate – slpm/scfh
Hot
222 / 470
Cold
250 / 530
Metric
Material
Thickness
Torch-to-Work
Distance
Initial Pierce Height
Pierce
Delay Time
Best Quality Settings
Production Settings
Cut Speed
Voltage
Cut Speed
Voltage
mm
mm
mm
%
seconds
mm/min
volts
mm/min
volts
2
1.5
3.8
250
0.1
7405
119
9970
121
3
0.2
6120
120
8240
122
4
0.5
4840
122
6110
123
6
2275
125
2840
125
8
0.7
1505
127
1860
127
10
4.5
300
1115
130
1245
128
12
1.2
720
133
925
130
16
Edge Start
465
137
505
136
20
320
141
345
141
English
Material
Thickness
Torch-to-Work
Distance
Initial Pierce Height
Pierce
Delay Time
Best Quality Settings
Production Settings
Cut Speed
Voltage
Cut Speed
Voltage
inches
inches
inches
%
seconds
ipm
volts
ipm
volts
16 GA
0.06
0.15
250
0.1
316
118
425
120
10 GA
220
121
296
122
3/16
0.2
152
123
168
123
1/4
0.5
72
125
96
125
3/8
0.7
48
130
52
128
1/2
0.18
300
1.2
23
134
32
131
5/8
Edge Start
19
137
20
136
3/4
14
140
15
140