8. Veneering

• 

Layering technique: 

Apply a thin layer of adhesive paste to the surfaces to be veneered and fire.  

(See below for firing instructions)

•  The HeraCeram materials are then layered and fired according to the HeraCeram user instructions.

• 

Stain technique: 

The restoration must be clean and grease-free. A roughened surface is of advan-

tage.

• Personalize restorations with HeraCeram Stains universal and fire. For more intense chromatic 

results, the procedure can be repeated.

•  Finally, glaze with HeraCeram Glaze universal and fire.

• 

Firing procedure: 

Veneers and inlays are positioned and fired on the smallest possible piece of firing 

wool placed of top firing pins.

•  Crowns are fired on suitable firing pins, fan pins, special firing wires or pins with adapted platinum 

foil or firing wool.

Firing recommendations

The firing temperatures given are intended as guidelines. Deviations are possible due to 

varying furnace performance.

General 

 Firing 

 Programme

Pre-heat  

or start 

 temperature

Pre-dry  

and pre-heat 

time

Heat rate

Final 

 temperature

Holding  

time

Vacuum  

start

Vacuum  

stop

 

°C

min

°C/min

°C

min

°C

°C

Adhesive

600

5

100

860

1

600

860

Stain and 

glaze firing

using Stains / 

Glaze 

 universal

600

6

100

860

0,5 – 1

Please follow our detailed processing instructions for processing of HeraCeramPress and the 

instructions in our safety data sheet.

Safety instructions:

Hypersensitivity to the product or its components cannot be ruled out in individual cases – in a sus-

pected case, please contact the manufacturer with regard to the ingredients. In the case of a suspected 

allergy, an allergy test is recommended before treatment. The data indicated corresponds to the best 

of our knowledge and is based on internal investigations. Do not swallow or consume this product. 

Avoid contact with the eyes. If the product does come into contact with the eyes, rinse them thoroughly 

with plenty of water immediately and consult an ophthalmologist. 
If you wish to contact us with regard to the product, please always indicate the lot designation.
Designation lot 

 : See note on packaging.

Dated: 2018-11

1809_15440_GBA_HeraCeram_Press.indd   7

21.12.18   10:24

Summary of Contents for HeraCeramPress

Page 1: ...ja obs ugi 20 HeraCeramPress Dateiname 1809_15440_GBA_HeraCeram_Press HK Toolbox Nr W19958 Ma e Falzma 148x210mm SAP Nr Version 99001313 12 ORT Version 07 Print PDF Datum HKG Freigabe am 21 12 2018 21...

Page 2: ...hnik zweckbestimmt sind Schichttechnik Modellationen m ssen eine Mindestst rke von 0 8 mm haben Pr molaren f r die Schichttechnik verkleinerte anatomische Form Okklusalprofil modellieren Ger stst rke...

Page 3: ...30 15 8 abh ngig vom Ofentyp 7 Ausbetten Die Lage der Pressobjekte mit Hilfe eines Pressstempels ermitteln und anzeichnen Danach die Ein bettmasse mit einer Trennscheibe auf H he des Pressstempels tie...

Page 4: ...m glich Allgemeines Brenn programm Vorw rm bzw Start temperatur Vortrocken und Vor w rmzeit Temperatur anstieg End temperatur Haltezeit Vakuum Start Vakuum Stop C min C min C min C C Adhesive 600 5 1...

Page 5: ...hick minimum Premolars reduced anatomical shape occlusal profile for the layering technique Framework thickness should be at least 50 of the total thickness For molar crowns the stain technique is to...

Page 6: ...on type of furnace 7 Deflasking Determine and mark the position of the pressed objects with the aid of a press plunger Then make a deep cut into the investment material with a cut off wheel at the en...

Page 7: ...r start temperature Pre dry and pre heat time Heat rate Final temperature Holding time Vacuum start Vacuum stop C min C min C min C C Adhesive 600 5 100 860 1 600 860 Stain and glaze firing using Stai...

Page 8: ...anat mica perfil oclusal reducida para la t cnica de estratificaci n El grosor de la estructura debe ser al menos el 50 del grosor total Para las coronas molares utilice la t cnica de maquillaje 3 Col...

Page 9: ...la inyecci n Tempera tura inicial Inicio del vac o Final del vac o Vac o Velocidad de calenta miento Tempera tura final Espera Inyecci n Presi n inyecci n C C C hPa C min C min min bar 700 700 1030 3...

Page 10: ...s con plataformas de platino o guata refractaria Recomendaciones de cocci n Las temperaturas de cocci n indicadas son orientativas Los valores pueden variar como consecuencia de los diferentes rendimi...

Page 11: ...per modellazione e isolanti completamente cal cinabili indicati per la tecnica della pressatura Le modellazioni per la tecnica della stratificazione devono avere uno spessore minimo di 0 8 mm Premola...

Page 12: ...eramPress Inserire il pistone monouso o di ossido di alluminio Posizionare velocemente nel forno di pressatura il cilindro cos caricato e avviare il programma di pressatura Al termine del programma di...

Page 13: ...otto Successivamente stratificare e cuocere le masse HeraCeram secondo le istruzioni per l uso HeraCeram Tecnica della colorazione il restauro deve essere perfettamente pulito e sgrassato Una superfic...

Page 14: ...sono al meglio delle nostre conoscenze e si basano su risultati di test condotti internamente Non ingerire questo prodotto Evitare il contatto con gli occhi Se il prodotto viene a contatto con gli occ...

Page 15: ...Pr molares contorno anat mico perfil oclusal reduzido para a t cnica de estratifica o A espessura da estrutura deve ter pelo menos 50 da espessura total Pode se usar a t cnica de maquiagem para coroa...

Page 16: ...aqueci mento Tempe ratura final Espera Prensa gem Press o de pren sagem C C C hPa C min C min min bar 700 700 1030 30 50 1030 15 8 depende do tipo de forno 7 Demuflagem Determine e marque a posi o dos...

Page 17: ...cadas como diretrizes Desvios s o poss veis devido varia o da pot ncia do forno Programa geral de queima Preaqueci mento ou temperatura inicial Tempo de pr secagem e preaqueci mento Aumento da tempera...

Page 18: ...mm Premolaarit pinnan anatomisen muodon purupinnan profiili on oltava matalampi jos k ytet n kerrostustekniikkaa Rungon paksuuden on oltava v hint n 50 kokonaispaksuudesta V rj ystekniikkaa on k ytet...

Page 19: ...C C C hPa C min C min min bar 700 700 1030 30 50 1030 15 8 uunin tyypin mukaan 7 Purseen poisto M rit ja merkitse puristettavien kohteiden asento puristuspistimen avulla Tee panostusmateriaa liin viil...

Page 20: ...sesti Yleinen poltto ohjelma Esil mmitys tai aloitus l mp tila Esikuivaus tai esil mmi tysaika L mp tilan nosto Lopullinen l mp tila Pitoaika Tyhji n aloitus Tyhji n lopetus C min C min C min C C Kii...

Page 21: ...do techniki t oczenia Odbudowa technik nak adania warstw musi mie grubo co najmniej 0 8 mm Z by przedtrzonowe na potrzeby techniki nak adania warstw nale y modelowa zredukowany kszta t anatomiczny Gr...

Page 22: ...w czy program t oczenia Po t oczeniu wyj mufl z pieca do t oczenia i pozostawi do ostygni cia do temperatury pokojowej Nale y unika stygni cia mufli pomi dzy wyj ciem z pieca do wst pnego podgrzewani...

Page 23: ...do wypalania z dopasowan foli platynow lub podk adkach do wypalania Zalecenia dotycz ce wypalania Podane temperatury wypalania maj s u y jako wytyczne Mo liwe s odchylenia ze wzgl du na zr nicowan mo...

Page 24: ...99001313 12 Manufacturer Kulzer GmbH Leipziger Stra e 2 63450 Hanau Germany Made in Germany 1809_15440_GBA_HeraCeram_Press indd 24 21 12 18 10 24...

Reviews: