Energy Settings
Arc Welding
The following settings may be used as a guide. The correct
setting for a particular metal combination and wire gauge will
produce a spherical bead.
A flattened bead indicates that the energy setting is too high.
Wire Diameter (mm)
Switch at “LOW”
0.1
Switch at “HIGH”
0.3
0.15
0.5
0.2
0.7
0.25
0.8
Electrodes
To replace or adjust carbon electrode, first turn the welder on
its side and slacken screw on base of argon shield, which may
be then pulled off. This reveals grub screw which holds carbon
electrode in place.
-
9
-