ENGLISH
TROUBLESHOOTING
TROUBLE ! MATERIAL RUNS OR DRIPS.
WHAT’S WRONG?
WHAT TO DO…
Spraying too much material.
Reduce paint flow by turning material adjustment knob.
Spraying too slowly.
Increase speed of application.
Spraying too close.
Increase distance from surface.
Viscosity too thin.
Check dilution recommendation.
TROUBLE! MATERIAL DRIPS FROM NOZZLE
WHAT’S WRONG?
WHAT TO DO…
Nozzle loose.
Screw nozzle tight.
Nozzle breaks.
Change
Y-type seal ring of nozzle breaks.
Change
Material accumulated /clog inside nozzle.
Clean
TROUBLE! TOO MUCH OVER SPRAY.
WHAT’S WRONG?
WHAT TO DO…
Sprayer too far from surface.
Reduce distance to surface.
Too much material being sprayed.
Reduce paint flow by turning flow control knob.
TROUBLE! LITTLE OR NO MATERIAL BEING RELEASED.
WHAT’S WRONG?
WHAT TO DO…
Spray nozzle/tip clogged.
Clean nozzles.
Y-type seal ring of nozzle missing.
Add seal ring to nozzle and assemble in place.
Pickup tube loose or clogged.
Check tube.
Canister loose.
Screw canister tightly in place.
Quick refill lid loose.
Screw quick refill lid tight in place.
Spray gun unit not fully attached to the power unit.
Check attachment of spray gun unit.
Flow control knob setting too low.
Increase flow control setting.
Air inlet blocked.
Clean or change air filter.
Material too thick.
Thin material per manufacturer recommendation.
TROUBLE! MATERIAL BEING SPRAYED IS SPLATTERING
WHAT’S WRONG?
WHAT TO DO…
Viscosity of material is too high.
Thin material per manufacturer recommendation.