7.0 Metallographic Cutting Basics
21
Philosophy:
1.
Cutting is the most important metallographic sample preparation step
2.
Minimize damage during sectioning
3.
Less sectioning damage = reduced number of grinding and polishing steps
Note: I
n some cases cutting damage cannot be removed by subsequent polishing operations
(especially for brittle samples)
Time Well Spent:
1.
Spend more time on sectioning in order to decrease overall sample preparation time
2.
Protect integrity of the specimen with proper sectioning
Wheel feed
-
High speed (3500 rpm)
-
High load (10 amps)
Table feed
-
Low speed (1500 rpm)
-
Low load (3 amps)
Finer finish with
minimal cutting burr
Coarse finish with
large cutting burr