WARNING: Handle lithium batteries 

carefully, observe warnings on battery casing. 

Dispose of in accordance with local regulations. 

 

RECONDITION PROCEDURE 

Exposure of the internal sensor to chemical vapours 

may  interfere  with  the  internal  sensor  and  cause 

inaccurate  readings  to  be  logged.  In  a  clean 

environment,  this  will  slowly  rectify  itself.  However, 

exposure to extreme conditions or chemical vapours 

will require the following reconditioning procedure to 

bring the internal sensor back to calibration state. 

80°C (176°F) at<5%RH for 36h (baking) followed by 

20-30°C (70-90°F) at>74%RH for 48h (re-hydration) 

High  levels  of  pollutants  may  cause  permanent 

damage to the internal sensor. 

 