08/10/2003
CT104 Manual
Tri-M Engineering
Tel:
800.665.5600, 604.945.9565
1407 Kebet Way, Unit 100
Fax:
604.945.9566
Port Coquitlam, BC V3C 6L3
E-mail:
info@tri-m.com
Canada
Web
site:
www.tri-m.com
7
For the VM method, the PC/104 stack is mounted to a vertical divider, CT6-VD00 or
CT8-VD00. The vertical divider with the PC/104 stack installed is then slid into the
vertical card slots in the Can-Tainer™ case. Accessory equipment, such as batteries and
transmitters, may be attached to the opposite side of the vertical divider.
CHAPTER 3: Can-Tainer Material Specifications
3.1 Aluminum Housing Materials
Alloy
- 6063-T5 Aluminum Extrusion
Finish
- Black Anodized. Other finishes available.
Table C:
Typical Properties of 6063-T5 Aluminum Extrusion Alloy*
Physical Property
Value
Average Coefficient of Thermal
Expansion
13.0 µin/°F (68° - 212 °F)
Approximate Melting Range
1140°F - 1210°F
Thermal Conductivity
1450 BTU - in/ft² hr °F (@
77°F)
Electrical Resistivity
2.8 µOhm-cm (@ 68°F)
Ultimate Strength
27,000 PSI
Yield Strength
21,000 PSI
Elongation
12%
(% in 2 in, 1/16" thick
specimen)
Hardness Brinell No.
60
(500 kg load, 10 mm ball)
Ultimate Sheer Strength
17,000 PSI
Fatigue Endurance Limit
10,000 PSI
(500 x 106 cycles Moore
Mach.)
Modulus of Elasticity
10 (106 PSI)
* Source: Aluminum Standards and Data, 1988 Aluminum
Association Inc.