20
-
2. Operation procedure
:
1). 2-step:
push torch trigger
pre-gas flow
arc start arc start current
DC Constant TIG
up-slope normal welding DC pulse TIG
AC constant TIG
AC pulse TIG
release trigger down-slope
crater filling
post-gas flow
end welding
2). 4-step:
push torch trigger
pre-gas flow
arc start arc start current
DC Constant TIG
release trigger
up-slope
normal welding
DC pulse TIG
AC constant TIG
AC pulse TIG
push torch trigger
down-slope
crater filling
release trigger
post-gas flow
end welding
TIG welding parameters for Al and Al-Mg alloy (Only for reference)