13.1.2
Preparing Tungsten for DC Electrode Negative (DCEN) Welding
The electrode should be pointed (tapered) according to the welding current.
Grind end of tungsten on fine grit, hard abrasive wheel before welding. Do not use wheel for other jobs
or tungsten can become contaminated causing lower weld quality.
Rule of thumb is that the taper section should be 2.5 times the Electrode Diameter.
Figure 69
Ideal Tungsten Preparation = Stable ARC
Diameter of the flat left on the end of the Electrode determines amperage capacity.
Figure 70
Wrong Tungsten Preparation = Wandering ARC
Figure 71
Pointing the Tungsten Electrode
The electrode should be pointed according to the welding current.
Figure 72
Electrode Angles
Angle @
Range of Current (Amps)
30°
0 – 30
60-90°
30 -120
90-120°
120 - 250
120°
≥250
Table 20
Summary of Contents for WeldForce WF-205MST
Page 36: ... 36 Weldclass 2019 E O E Edition 2 1 Figure 25 ...
Page 37: ...WF 205MST Weldclass 2019 E O E Edition 2 1 37 8 6 Primary Schematic Circuit Diagram Figure 26 ...
Page 42: ... 42 Weldclass 2019 E O E Edition 2 1 Figure 33 Figure 34 Figure 35 Figure 36 ...
Page 77: ...WF 205MST Weldclass 2019 E O E Edition 2 1 77 NOTES ...
Page 78: ... 78 Weldclass 2019 E O E Edition 2 1 ...
Page 79: ...WF 205MST Weldclass 2019 E O E Edition 2 1 79 ...
Page 80: ... 80 Weldclass 2019 E O E Edition 2 1 www Weldclass com au WF 205MST ...