13.5 Adjustment of Pulse Welding Characteristics
13-8
HW0480311
HW0480311
13.5.2
Adjustment of MIG Pulse Welding Characteristics
The following parameters change the pulse welding characteristics under the main character-
istics for aluminum MIG welding.
Parameter
No.
Meaning
Guideline of Adjustment
P08
Pulse peak current for droplet transition
-For excessive spatters;
Increase the value.
-For excessive burning;
Decrease the value.
P09
Base current to keep arc
P10
Pulse peak time for droplet transition
P35
Pulsed current increasing rate
-For arc repelling; Increase the value.
-For arc burning; Decrease the value.
P36
Pulsed current decreasing rate
Base current
Pulse time
Pulse current decreasing rate
Pulse current
Base
current
Droplet
transition
Pulse
current
Pulse current increasing rate
P10
P35
P09
P08
P36
I
t
101/129