Our products are manufactured in compliance with: CEI 46-1 (construction parameters); EN 50117(screening efficiency); CEI EN 50289(SA test methods); IEC 60332-1-2(cables with LSZH jacket)

HyperFlex 5

/.212

/.212

"

"

Crystal clear PVC jacket.

PVC Ø 5,4 mm ± 0,15

(0.212 inches ± 0.0059)

SRL

0,3-600 MHz >28 dB

600-1200 MHz >25 dB

1200-2000 MHz >22 dB

ATTENUATION at 20°C/68°F

FREQUENCY dB/100m dB/100ft

1,8 MHz

1,48

0,45

3,5 MHz

1,91

0,58

7,0 MHz

2,33

0,71

10 MHz

2,63

0,80

14 MHz

3,04

0,93

21 MHz

3,64

1,11

28 MHz

4,16

1,27

50 MHz

5,58

1,70

100 MHz

8,02

2,44

144 MHz

9,66

2,94

200 MHz

11,44

3,49

400 MHz

16,37

4,99

430 MHz

17,0

5,18

800 MHz

23,48

7,16

1000 MHz

26,46

8,07

1296 MHz

30,5

9,30

2400 MHz

42,58

12,98

3000 MHz

48,1

14,66

4000 MHz

56,95

17,36

5000 MHz

65,29

19,90

6000 MHz

72,92

22,23

POWER HANDLING (at 40°C/104°F)

FREQUENCY MAXP

FREQUENCY MAXP

1,8 MHz 1274 W

400 MHz 115 W

3,5 MHz 987 W

430 MHz 111 W

7,0 MHz 809 W

800 MHz 80 W

10 MHz 717 W

1000 MHz 71 W

14 MHz 620 W

1296 MHz 62 W

21 MHz 518 W

2400 MHz 44 W

28 MHz 453 W

3000 MHz 39 W

50 MHz 338 W

4000 MHz 33 W

100 MHz 235 W

5000 MHz 29 W

144 MHz 195 W

6000 MHz 26 W

200 MHz 165 W

Inner conductor made of 19x0,29 stranded geometric

and concentric copper wires. Purity 99,99% annealed.

(annealed = thermal softening process)

Cu 19x0,29 mm - Ø 1,4 mm 

± 0,15

(19x0.011 inches - 0.055 inches 

± 0.0059

)

ELECTRICAL DATA

Impedance @200MHz :

50 Ohm ± 3

Minimum bending radius:

Multiple bends/single bend

50/25 mm

(1.97/0.98 in)

Temperature:

-45°C to + 70°C (-49°F to +158°F)

Capacitance:

74 pF/m ± 2

(22.6 pF/ft ± 2)

Velocity ratio:

87 %

Screening efficiency:

100-2000 MHz

>105 dB

Class

A++

Inner conductor resistance: 14 Ohm/Km

(4.3 Ohm/1000ft)

Outer conductor resistance: 11 Ohm/Km

(3.4 Ohm/1000ft)

Tension test (spark test):

4 kV

Weight (100m/100ft):

4,2 Kg

(9.25 lb)

Maximum peak power:

2900 WATT

Connectors: C.N.HF5M-S ; C.BNC.AC5M-S ; C.UHF.AC5M-S

High resistance copper screen 

(Cu)

made by means

of 

24 spools

braiding machines. (50% more crosso-

vers if compared to traditional 16 spools machines.)

This  braid  is

HIGHLY  EFFECTIVE AGAINST

IMPULSIVE NOISES.

SCREENING PERCENTAGE: 88% 120 wires

High pressure physical injection

foamed polyethylene.

TRIPLE LAYER DIELECTRIC

FPE Ø 3,7 mm

± 0,05

(0.145 inches 

± 0.05

)

The copper foil has an applied PE-

coating, placed in order to prevent  foil

cracking due to short radius bends.

SCREENING PERCENTAGE 100%

CU-POL

Pb

RoHS

COMPLIANT

2002/95/EG

UV resistant black PVC jacket.

PVC Ø 5,4 mm

± 0,15

(0.212 inches

± 0.0059

)

HyperFlex 5

Crystal

/.212

/.212

"

"

Datasheets_Layout 1  09/05/2017  10:17  Pagina 16

 6

For step by step assembly instructions of connectors, please visit our website www.messi.it

Reviews: